The industry standard for hardness the hardness of a wood is rated on an industry wide standard known as the janka test.
Janka hardwood scale.
The test involves measuring the force required to embed a 444 steel ball into wood to half its diameter.
The janka rating is given in pounds force lbf by measuring how much force is needed to imbed a standard sized steel ball halfway into the wood.
Woods with a higher rating are harder than woods with a lower rating.
It is also a good indicator of how hard a.
The janka test is a measure of the hardness of wood.
The janka hardness test was conducted by measuring the amount of force necessary to embed a 444 inch steel ball into side of the wood up to one half of its diameter to determine its hardness rating which is then recorded on the janka hardness scale.
Janka hardness scale for hardwood flooring the janka hardness test was designed to rate the relative hardness of wood on a scale of 0 to 4000.
The janka scale is used to determine the relative hardness of particular domestic or exotic wood species.
The janka hardness scale is a test to rate the relative hardness of a wood flooring.
The scale was invented in 1906 by gabriel janka an austrian wood researcher and standardized in 1927 by the american society for testing and materials depending on the room where the flooring will be installed a certain level of hardness may make it a more desirable choice.
This test is one of the best measures of the ability of a wood specie to withstand denting and wear.
The janka test measures the amount of force required to embed a 0 444 steel ball into the wood to half of its diameter.
The test measures the force required to push a steel ball with a diameter of 11 28 millimeters 0 444 inches into the wood to a depth of half the ball s diameter.
For hardwood flooring the test usually requires a 2 6 sample with a thickness of at least 6 8mm and the most commonly used test is the astm d1037.
We ll be with you every step of the way ensuring that each stage of the project is a success.
When testing wood in lumber form the janka test is always carried out on wood from the trunk of the tree known as the heartwood and the standard sample according to astm d143 is at 12 moisture content and clear of knots.
The janka test was developed as a variation of the brinell hardness test.